华南理工大学学报(自然科学版) ›› 2012, Vol. 40 ›› Issue (7): 135-141.

• 材料科学与技术 • 上一篇    下一篇

动态硫化TPEE /ACM/纳米SiO2复合材料的制备

卢珣 林艳梅 吴叔青 田敏   

  1. 华南理工大学 材料科学与工程学院,广东 广州 510640
  • 收稿日期:2011-12-16 修回日期:2012-03-02 出版日期:2012-07-25 发布日期:2012-06-01
  • 通信作者: 卢珣(1969-) ,男,博士,副教授,主要从事高分子材料改性研究 E-mail:luxun@ scut.edu.cn
  • 作者简介:卢珣(1969-) ,男,博士,副教授,主要从事高分子材料改性研究
  • 基金资助:

    国家自然科学基金资助项目( 21073066)

Preparation of TPEE/ACM/Nano-SiO2 Composite via Dynamic Vulcanization

Lu Xun  Lin Yan-mei  Wu Shu-qing  Tian Min   

  1. School of Materials Science and Engineering,South China University of Technology,Guangzhou 510640,Guangdong,China
  • Received:2011-12-16 Revised:2012-03-02 Online:2012-07-25 Published:2012-06-01
  • Contact: 卢珣(1969-) ,男,博士,副教授,主要从事高分子材料改性研究 E-mail:luxun@ scut.edu.cn
  • About author:卢珣(1969-) ,男,博士,副教授,主要从事高分子材料改性研究
  • Supported by:

    国家自然科学基金资助项目( 21073066)

摘要: 将热塑性聚醚酯弹性体( TPEE) 和丙烯酸酯橡胶( ACM) 共混动态硫化制成一种耐油、耐热的热塑性硫化胶( TPEE /ACM TPVs) ,并在制备TPEE /ACM TPVs 的过程中添加不同量的纳米SiO2,研究了TPEE /ACM 共混比和纳米SiO2 对TPEE /ACM TPVs 动态力学性能、流变性能、力学性能、热稳定性能、耐热老化性能和耐热油性能的影响.研究结果表明: 当TPEE /ACM 共混比为60 /40 时,TPVs 的综合性能较好; 纳米SiO2 使TPVs 的加工性能变差; TPVs 只有一个玻璃化转变温度,纳米SiO2 提高了TPVs 的玻璃化转变温度; 当纳米SiO2 添加量为20% ( 质量分数) 时,TPVs 的综合力学性能较好; 当纳米SiO2 添加量为10%或20%时,TPVs 的耐热老化性能和耐热油性能较好.

关键词: TPEE /ACM 热塑性硫化胶, 动态硫化, 纳米SiO2, 流变性能, 耐热油性能

Abstract:

By using thermoplastic polyeher ester elastomer ( TPEE) and acrylate rubber ( ACM) as the raw materials,thermoplastic vulcanizate composites with oil and thermal resistance,namely TPEE/ACM TPVs,were prepared via a dynamic vulcanization at different nano-SiO2 dosages. Then,the dynamic mechanical property,the rheological behavior,the thermal stability,the heat-aging property and the heat oil resistance of the product were investigated
at different TPEE /ACM ratios and nano-SiO2 dosages. The results show that TPEE /ACM TPVs with high performance can be produced when the TPEE /ACM ratio achieves 60 /40,that the processability of TPVs becomes poor with the addition of nano-SiO2,that TPVs has only one glass transition temperature that increases after the addition of nano-SiO2,that the TPVs with a nano-SiO2 dosage of 20% ( mass fraction) is of high performance,and that better heat-aging property and strong heat oil resistance may obtained when the nano-SiO2 dosage varies from 10% to 20%.

Key words: TPEE /ACM thermoplastic vulcanizate, dynamic vulcanization, nano-SiO2, rheological behavior, hot oil resistance

中图分类号: