Journal of South China University of Technology (Natural Science Edition) ›› 2019, Vol. 47 ›› Issue (1): 48-55.doi: 10.12141/j.issn.1000-565x.180107

• Architecture & Civil Engineering • Previous Articles     Next Articles

Static Tensile Behavior of Half Grout Sleeve Splicing of Rebars Under High Temperature
 

 ZHANG Wangxi1, 2 DENG Xi2 HE Chao2   

  1.  1. Hunan Provincial Key Lab on Diagnosis for Engineering Structures,Hunan University,Hunan 410082,Changsha,China; 2. College of Civil Engineering,Hunan University,Changsha 410082,Hunan,China
  • Received:2018-03-12 Revised:2018-06-20 Online:2019-01-25 Published:2018-12-01
  • Contact: 张望喜( 1971) ,男,博士,副教授,主要从事装配式混凝土结构及防连续倒塌研究 E-mail:wxizhang2000@163.com
  • About author:张望喜( 1971) ,男,博士,副教授,主要从事装配式混凝土结构及防连续倒塌研究
  • Supported by:
    Supported by the National Program on Key Basic Research Project of China( 2016YFC0701400) and the National Natural Science Foundation of China( 51578228) 

Abstract:  The static tensile test was carried out for 12 half grout sleeve splicing of rebars specimens under high temperature,and 12 steel bars in the same batch were tested as control group under the same conditions. The influence of the temperature on the specimens and the mechanical property difference between the specimens and the steel bars under high temperature were studied. The test results show that the ultimate tensile strength of the specimens is similar to that of the steel bar under high temperature,and the failure modes of the specimens are the tensile rupture of rebars and the pulling-out of rebars. The tensile behaviors of the specimens are similar to the constitutive relations of uniaxial tension of the steel bars at temperatures of 200℃ and below,while the mechanical properties of the specimens is different from those of the steel rebars at temperatures of 400℃ and above. The failure modes of the specimens at room temperature and 400℃ are both tensile rupture of rebars. At 600℃,the rebars of the specimens may be pulled out first,rather than be ruptured. 

Key words: half grout sleeve splicing of rebars, rebar, static tensile, mechanical property, failure mode

CLC Number: