Infiltrants for Post-Processing of Three-Dimension Printing Specimens

Cheng Jiang1 Wu Jiao-jiao1 Xu Shou-ping1 Zhou Dong-wei2 Zhou Liang3   

  1. 1. School of Chemistry and Chemical Engineering,South China University of Technology,Guangzhou 510640,Guangdong,China;2. Foshan Heyu Chemical Co. ,Ltd. ,Foshan 528313,Guangdong,China; 3. Department of Light Chemical Engineering,Guangdong Industry Technical College,Guangzhou 510300,Guangdong,China
  • Received:2014-07-01 Revised:2014-09-05 Online:2015-02-25 Published:2014-12-31
  • Contact: 程江(1965-),男,博士,教授,主要从事精细化工研究. E-mail:cejcheng@scut.edu.cn
  • About author:程江(1965-),男,博士,教授,主要从事精细化工研究.
  • Supported by:
    Supported by the Project of Integration of Industry,Education and Research of Guangdong Province and Ministry of Education of China(2012B091100442)

Abstract: This paper deals with the water resistance,compressive strength,dimensional deviation and surficial mi-crostructure of gypsum-based three-dimension printing specimens affected by filling enhancers(namely infiltrant A),base materials of infiltrant B,dosage of waterborne epoxy emulsion in infiltrant B and immersion time. The re-sults show that(1) nano-silicone superhard curing agent is the most suitable enhancer for infiltrant A because it sig-nificantly improves the compressive strength of printing specimens; (2) waterborne polyurethane emulsion PU-202B is the most appropriate base material of infiltrant B; (3) the addition of waterborne epoxy emulsion in infiltrant B improves the compressive strength and water resistance of printing specimens,but excess waterborne epoxy emulsion may result in a dimensional deviation of the specimens; (4) the best immersion time for the three-dimension print-ing specimens into infiltrants A and B is 130s and 35s,respectively; and (5) after being immersed in infiltrant A and subsequently in infiltrant B,the specimens are of high compressive strength,weak water absorption,smooth surface and strong bond capability.

Key words: three-dimension printing, printing specimen, post-processing infiltrant, compressive strength, water absorption