华南理工大学学报(自然科学版) ›› 2014, Vol. 42 ›› Issue (10): 95-101.doi: 10.3969/j.issn.1000-565X.2014.10.016

• 化学化工 • 上一篇    下一篇

添加流变助剂的烟草薄片性能

高文花1,2 陈克复1 杨仁党1 杨飞1†   

  1. 1.华南理工大学 制浆造纸工程国家重点实验室,广东 广州510640;2.华南理工大学 环境与能源学院,广东 广州510006
  • 收稿日期:2014-01-10 修回日期:2014-06-23 出版日期:2014-10-25 发布日期:2014-10-01
  • 通信作者: 杨飞(1978-),男,博士,副研究员,主要从事纸页成型与加工(特种纸与加工纸)研究. E-mail:yangfei@scut.edu.cn
  • 作者简介:高文花(1987-),女,博士后,主要从事植物资源综合利用研究.E-mail:gaowenhua2010@gmail.com
  • 基金资助:

    “十二五”国家科技支撑计划重点项目(2013BAC01B03);华南理工大学中央高校基本科研业务费专项资金资助项目(2014ZB008,2014ZZ0062);华南理工大学制浆造纸工程国家重点实验室2013年开放基金资助项目(201310)

Properties of Reconstituted Tobacco with Rheological Additives

Gao Wen-hua 1, 2  Chen Ke-fu 1  Yang Ren-dang 1  Yang Fei 1   

  1. 1. State Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou 510640, Guangdong, China;2. College of Environment and Energy, South China University of Technology, Guangzhou 510006, Guangdong, China
  • Received:2014-01-10 Revised:2014-06-23 Online:2014-10-25 Published:2014-10-01
  • Contact: 杨飞(1978-),男,博士,副研究员,主要从事纸页成型与加工(特种纸与加工纸)研究. E-mail:yangfei@scut.edu.cn
  • About author:高文花(1987-),女,博士后,主要从事植物资源综合利用研究.E-mail:gaowenhua2010@gmail.com
  • Supported by:

    “十二五”国家科技支撑计划重点项目(2013BAC01B03);华南理工大学中央高校基本科研业务费专项资金资助项目(2014ZB008,2014ZZ0062);华南理工大学制浆造纸工程国家重点实验室2013年开放基金资助项目(201310)

摘要: 涂布工艺是造纸法烟草薄片加工过程中的核心技术之一。通过添加流变助剂CMC、GG-50、CGG于涂料中,调整涂料性质,改善涂布工艺,分析流变助剂添加与涂布加工后薄片性质之间的关系。研究表明:,随着流变助剂添加量的增大,涂料的黏度增高,涂布后烟草薄片的松厚度、透气度和填充值降低,而抗张强度和撕裂指数提高,主流烟气中焦油、总粒相物和一氧化碳的释放量增高。涂布后薄片的SEM分析表明:,当3种流变助剂的用量均为0.1%时,薄片表面呈现较好的涂层结构,涂料均匀填充于薄片纸基内部,且涂层表面没有片状结构生成。

关键词: 流变助剂, 烟草薄片, 涂料, SEM, 主流烟气

Abstract:

The coating process is one of the core technologies forin the manufacture of reconstituted tobacco. In the investigation, three rheological additives, namely CMC, GG-50 and CGG, were respectively added into the coating to adjust the coating properties and improve the coating process. Then, the relationship between the additives and the properties of the reconstituted tobacco after coating is discussed. The results show that (1) with the increase of the rheological additive dosage, the coating viscosity and the tensile strength and the tear index of the reconstituted tobacco after coating increase while the bulk, the air permeability and the filling value of the reconstituted tobacco after coating decrease; (2), simultaneously, the release amounts of tar, total particulate matter and carbon monoxide in the main smoke also rise. The SEM analysis of reconstituted tobacco shows that when all the dosages of the three rheological additives are all 0.1%, the coating structure on the reconstituted tobacco surface is better, , the coating fills in the inside of reconstituted tobacco base-paper, and there is no fragment on the coating surface.

Key words: rheological additive, reconstituted tobacco, coatings, SEM, main smoke