Analysis of Key Parameters of Non-Tension Prestressing Technology for Continuous Steel-Concrete Composite Beams

Expand
  • 1.State Key Laboratory for Geomeehanics and Deep Underground Engineering,China University of Mining and Technology(Beijing),Beijing 100083,China;2.Department of Civil EngineeringfKey Laboratory of Civil Engineering Safety and Durability of the Education of Ministry,Tsinghua University,Beijing 100084,Chin
吴丽丽(1977-),女,博士,副教授,主要从事结构工程研究

Received date: 2010-04-21

  Revised date: 2010-08-30

  Online published: 2011-03-01

Supported by

国家自然科学基金资助项目(50778103,50808110);中国博士后科学基金资助项目(20080430042)

Abstract

By analyzing the loading stages of the continuous steel-concrete composite beams with 2-5 spans,some key parameters of the non-tension prestressing technology of the composite beams,such as the counterweights and their arrangement,as well as the post-cast length of concrete in the negative-moment region,are investigated.Then,the calculation methods of crack width in the negative-moment region and mid-span deformation of the composite beams are discussed after the removal of the counterweights.It is suggested that the reverse deflection induced by the non-tension prestressing can be obtained through two steps,namely,converting the reverse loads resulting from weight removing to the full-span uniform "equivalent" ones,and then calculating the deflections under the "equivalent" loads.With this two-step method,the requirements of practical engineering are satisfied well,and the maximum relative error of deflection keeps within 15%.

Cite this article

Wu Li-li Nie Jian-guo . Analysis of Key Parameters of Non-Tension Prestressing Technology for Continuous Steel-Concrete Composite Beams[J]. Journal of South China University of Technology(Natural Science), 2011 , 39(4) : 156 -162 . DOI: 10.3969/j.issn.1000-565X.2011.04.027